This was an ornament I printed roughly 6 years ago. Being a Christmas ornament it spent most of those 6 years stored in my roof space.

Being in Australia this would have been subject to average temperatures of 30 to 35 degrees c but also peaks across summer approaching 70 degrees c. Also in high humidity.

The PLA crumbles into tiny pieces at the softest touch.

I thought it was interesting that PLA would start to break down in these conditions.

  • ExcessShiv@lemmy.dbzer0.com
    link
    fedilink
    English
    arrow-up
    2
    ·
    2 months ago

    it will be readily metabolized by the various ubiquitous species populating our biosphere. i suppose it’s a good thing. possibly the only microplastic that doesn’t suck

    Not really, it is considered compostable in industrial composting conditions. It will not degrade at a reasonable timeframe in natural conditions and will basically just remain micro plastic.

    • unexposedhazard@discuss.tchncs.de
      link
      fedilink
      English
      arrow-up
      1
      ·
      2 months ago

      yep sadly PLA being ok for the environment is a big ol myth unless it is either turned back into filament or properly recycled / industrially composted